Guides/Installation and care

Terrazzo and moisture: let it dry first.

Italian terrazzo tile arrives holding water. Almost every problem we hear about comes from sealing it or covering it before that water has left. This is how we tell clients and tilers to handle it.

By Michael, Lulo TileUpdated November 20266 minute read
Italian terrazzo tile in Bianco
Italian terrazzo · Bianco
In short
  1. 01It arrives dampTerrazzo fresh off the boat still holds moisture. Get it to site early and let it dry.
  2. 02Seal the back before layingA back-seal keeps the adhesive water out, so the tile dries faster through its face.
  3. 03Seal the face lastOnly once the tile is dry and even in tone. Sealing early locks the moisture in.
  4. 04Mind where it goesYes to bathroom floors. Ask us about shower floors. Not around pools.
01

It arrives holding moisture.

Cement terrazzo is cast, cut and ground wet, then packed and shipped. It reaches Sydney with moisture still inside it.

There is always some residual moisture in the tiles when they are fresh off the boat.
Michael, Lulo Tile

You can see it. A damp tile looks darker and patchy, and it lightens and evens out as it dries. That change in tone is the best gauge you have, and nearly every step below waits on it.

Our advice is to get the tile on site sooner rather than later, so it can acclimatise and dry out fully before anyone lays it. Allow two to four weeks before laying where the program lets you. Unpack it and stand the tiles so air can get around them.

02

Two seals, two different jobs.

This is the part that gets misread most. There are two sealing operations on a terrazzo floor. They happen at different times and they do opposite things.

The back-seal, before laying

The underside and edges of each tile are sealed with Aqua Mix ProBlock before the tile goes down. This stops the mix water in the adhesive and grout soaking up into the tile, which means the tile only has to lose the moisture it already holds, and it dries faster through the top face. Allow about 1 litre of ProBlock for every 8 m².

Do not swap in an ordinary sealer for this step. A normal sealer on the back of a tile reduces how well the adhesive bonds. ProBlock is made so that it does not. The premium sealer is for the top face.

Tell your adhesive supplier

ProBlock is not a bond breaker, but it does reduce the porosity of the sealed face. Tell whoever specifies your adhesive that the tiles are back-sealed so they can specify to suit.

The face-seal, after laying

The top face is sealed with Aqua Mix Sealer's Choice Gold, and only once the floor is dry and even in tone. Seal it while it is still damp and you lock the moisture in. Allow 14 days after grouting as a minimum. Four to six weeks is more realistic.

If you have an older instruction sheet that names a "Rapid Cure" version of that sealer, it has been replaced by a new formulation. Follow the cure times on the tin you actually have.

03

Laying it.

  • Adhesive by type. A white, rapid-setting, low-water, deformable cement adhesive (class C2 F S1), with a flow bed for the large format. Less water in the bed means less water for the tile to take up.
  • Cut wet, never dry. Dry cutting throws crystalline silica dust.
  • Do not beat it in with a rubber mallet. Bed it by hand.
  • Grout the whole face. Terrazzo has pinholes. The grout is worked across the entire surface as a slurry so the pinholes fill, then cleaned back.
  • Pick a pale grey grout. Something like a misty grey sits quietly against most colours. Dark grout is harder to keep off the face.
  • In public areas, consider epoxy grout. It gives the best stain resistance.
  • Do not cover the floor after grouting. Drop sheets, cardboard and plastic trap the moisture and mark the tile. If it has to be protected, use something that breathes.
04

How much to order.

Order 15% over the measured area. Make it 20% for the Grande format, for patterned layouts and for rooms with a lot of cutting.

Order it all at once. The batches are not wildly different, but where tiles from one batch butt up against tiles from another, you can see a difference in colour balance. One order from one batch avoids the question.

It is also heavy. Allow about 49 kg per square metre, and around 17.5 kg for a single 600 × 600 mm tile. Plan the delivery and the lifting with that in mind.

05

Where it suits, and where it does not.

  • Living areas, kitchens and bathroom floors: yes.
  • Shower floors: ask us first, so we can talk through the finish and the fall.
  • Pool surrounds: no. Honed terrazzo is too slippery when wet for use around a pool.

We do not publish a slip rating for this terrazzo, because we do not hold a current test for it. If your project needs a rated floor, tell us at the start.

06

Efflorescence and everyday care.

If a white bloom appears on a new floor, it is efflorescence: salts carried to the surface by moisture leaving the tile. It is another sign the floor is still drying. Do not treat it with acid. Acid attacks the cement and the marble chip and leaves a mark you cannot polish out by hand.

Once the floor is sealed, clean it with a pH neutral cleaner. Keep acids, bleach and abrasive cleaners away from it, and wipe up wine, citrus and oil when they land.

We supply tile and stone. We are not installers. This article is general advice from our experience with clients and trades; your tiler and waterproofer remain responsible for the installation.

Questions

Before you order.

Why does my new terrazzo look patchy or dark?

It is still holding moisture. Terrazzo arrives damp and darkens where it is wet. The tone evens out as it dries, which takes weeks rather than days.

When can terrazzo be sealed?

The underside and edges are sealed before laying. The top face is sealed only once the floor is dry and even in tone: at least 14 days after grouting, and more often four to six weeks.

What is the white powder on my terrazzo floor?

Efflorescence: salts brought to the surface as moisture leaves the tile. It means the floor is still drying. Do not use acid on it.

Can terrazzo be used in a bathroom?

Yes on bathroom floors. Ask us before using it on a shower floor. We do not recommend it around pools, and we do not publish a slip rating for it.

How much extra terrazzo should I order?

15% over the measured area, or 20% for the Grande format, patterned layouts and cut-heavy rooms. Order it in one batch.

Visit the showroom

See the chip.

Book a showroom visit and we will put the terrazzo colours on the floor beside your other finishes.

Showroom · Northbridge, Sydney  ·  All guides and articles